Screed floor repair. Restoration technology for polymer and epoxy coatings

Compounds for self-leveling floors in our time are very widely used for fine leveling of the base for decorative flooring. They appealed to both professional builders and amateurs who want to do everything in their house on their own. Such popularity is explained by the fact that it is convenient to work with these building mixtures, they are well distributed over the surface and quickly harden, making it possible to quickly move on to subsequent stages of finishing.

But if during the preparation of the base, as well as during the preparation, pouring and distribution of the composition over the surface, the technology for performing work is violated, after the hardening of the floor or already during its operation, various kinds of defects may appear, including cracks. This, in the absence of work experience, unfortunately, happens quite often. And therefore the topic - "self-leveling floor repair of cracks" is very relevant.

This publication will consider several issues that may arise in such situations, including the possibility of getting rid of the problems that have arisen.

Causes of cracks

There can be many reasons for the occurrence of cracks in the self-leveling layer of the floor, and they are most often associated with a violation of manufacturing and installation technology. This may be an improperly prepared surface, an expired or cheap low-quality dry mix, high humidity, low or too high air temperature in the room, and more.


Cracks, blisters, delaminations - consequences of either the use of a low-quality mixture, or a violation of the work technology

Repairing defects and even more so reworking the entire floor is not an easy task. That is, it is better not to allow the appearance of flaws in principle. Therefore, it makes sense once again to dwell in more detail on the main points that determine the quality of the bulk coating.

  • Optimal temperature- this is one of the main conditions for obtaining high-quality coverage. Therefore, the manufacturer of the mixtures gives certain recommendations on the use of the material, which must be placed on the packaging. As a rule, the temperature range for operation varies between +5 and 30 degrees. But this is the limit, and it is best to pour at temperatures from 15 to 25 degrees.

This is due to the fact that at too low temperatures, the adhesive ability of the solution and the base material decreases, especially if their temperature is seriously different. Because of this, the bulk layer may begin to peel off from the concrete screed and crack.

If the solution is poured at elevated air temperatures, uneven setting and drying of the solution may occur, which will also lead to cracking of the coating.


  • Base humidity level can also cause defects on the flooded floor. Therefore, before starting work, it is necessary to check this parameter as well - it should be no more than 4%.

If the floors were recently leveled with a rough screed, then at least three or even four weeks should pass from the day it was laid, depending on the layer thickness and temperature. Only after this period, the concrete will gain enough strength, and excess moisture will leave it.

If you pour a self-leveling floor solution on an undried base, then the moisture not involved in the hydration process will definitely swell the finish layer when it dries, resulting in cracks.

Of course, not everyone has a moisture meter. But you can use another proven method to control the moisture content of the base.


A square sheet of polyethylene film (at least 100 µm thick) is cut out with sides of approximately 1000 × 1000 mm. It is spread on a concrete floor and attached to it around the perimeter with construction tape. In this position, this impromptu "measuring device" is left for a day. If after this period the film remains dry, you can fill it. But when traces of perspiration or, even worse, drops of condensate are visible, the concrete screed has clearly not yet reached the desired condition.

  • Failure to comply with the surface preparation technology for the self-leveling floor, will necessarily lead to deformation of the finish layer. The base must not only be dried well, but also, preferably, sanded. For this purpose, industrial or manual grinders are used.

During this process, the pores of the concrete structure are opened, which will contribute to the creation of high adhesive characteristics of materials. Further, the surface must be thoroughly cleaned from the remnants of dust and dirt, using a powerful vacuum cleaner for this. All grease, oil, bituminous stains will also have to be eliminated - they must be cleaned down to “healthy” concrete.

Self-leveling floor prices

self-leveling floor


  • Detergents. When preparing the base, in addition to a vacuum cleaner, cleaning agents are used to clean it, which should be a special acid - a converter of cement deposits. After surface treatment with this compound, it must be further sanded.

Do not use household detergents to clean concrete, as they are absorbed into the structure of the material, and it is impossible to remove them completely. The components that make up detergents can also lead to peeling and cracking of the self-leveling floor.

  • Lack of or poor-quality application of the primer composition- one of the common reasons for the sad results of pouring.

A properly primed base is always a prerequisite for a quality self-leveling floor.

The cleaned surface must be properly primed, and it is advisable to use the composition of the same manufacturer for this process, which is planned to level the base. The primer should be applied to the entire surface of the base - even very small areas should not be skipped. And it is better to do this process two or three times, waiting for each layer to dry. The primer will bind the concrete structure and create the prerequisites for good adhesion of the base and the self-leveling floor.

  • Repair of the base concrete screed. If the screed is old but in reasonably good condition, fine cracks may not be visible on it. But after grinding the surface or drying the primer layer, cracks may appear.

The self-leveling floor cannot be laid on such a base, so the screed must be repaired. This process can be carried out in the traditional way, that is, the crack is widened, primed and filled with concrete mortar or a more elastic and quickly hardening material, for example, one of the putties suitable for concrete repair


Sealing cracks with a special repair compound

Such repair compounds are very often offered by the same companies that produce mixtures for.

If the repair is carried out in the traditional way before applying the primer, then special solutions are used after it dries.


Repair of a screed with reinforcement of the surface with a sickle mesh

Some craftsmen use a sickle mesh to strengthen the screed, laying it on separate sections or completely on the entire surface.

If you do not repair the cracks on the base rough screed, they may appear through the layer of the self-leveling floor.

  • Incorrectly carried out application of self-leveling floor mortar. A violation of the technological process of mixing the solution, its pouring and distribution over the surface can lead to swelling and cracking of the self-leveling floor. Therefore, it is imperative to act, strictly following the manufacturer's recommendations placed on the packaging of the dry mortar.
  • Insufficient strength, leveling the base, screeds. If the rough screed is old, or is made of poor-quality mortar that does not have good strength after maturation, then the self-leveling floor will begin to quickly collapse. Therefore, the repair of an old draft screed or the arrangement of a new one should be carried out with maximum quality. If necessary, the old, unreliable screed is completely dismantled, and a new one is laid in its place.

Important rules for pouring concrete screed

In order for the base of the floor to be strong and reliable, you need to know how to approach its arrangement. It is this process that is described in detail in a special publication of our portal.

cement prices

  • Absence of a damper tape around the perimeter of the self-leveling floor. The technology for arranging any type of floor, whether it is a capital screed or a leveling bulk layer, requires the use of a damper tape, which is glued at the bottom of the wall around the entire perimeter of the floor.

Ignoring the laying of damper tape around the perimeter of the floor is to plant a “time bomb” in it

This material is designed to preserve surfaces from deformation and cracking, as it is able to compensate for the expansion processes of the material when temperatures change.

  • The layer thickness parameters are not respected. The manufacturer indicates in the characteristics of the mixture the permissible range of thicknesses of the self-leveling floor layer. If the recommendations are not followed, the coating may acquire a “cushion” effect, which will result in the delamination of the solidified solution from the base.
  • drafts. When filling and distributing the solution over the surface of the rough screed and during the solidification of the composition, all windows and doors are kept closed. Drafts must be completely excluded. Failure to comply with this rule may also well cause swelling and cracking.

How to repair a defective self-leveling floor?

It should be noted right away that it is not always possible to repair the self-leveling coating. In some cases, it is necessary to completely dismantle a low-quality layer and then, after carrying out comprehensive preparatory operations, equip a new one.

The first step after solidification of the bulk mixture distributed over the floor surface, it is necessary to revise this layer for any flaws.


If a crack or other defects are found, then you should not immediately begin to eliminate them. It is necessary to monitor their "behavior" for several days. Only after that it will be possible to make a decision on the tactics of further actions.


If the cracks have expanded and elongated, numerous branches have come from them, or other flaws have formed - delamination and swelling, which occupy more than 15% of the surface, then, unfortunately, the coating will have to be dismantled and the surface leveling work should be carried out again, starting from the preparation of the base.


If the defects are localized in separate areas and do not tend to expand and grow, then it is quite possible to repair the surface.

Crack repair

Crack repairs are carried out in the following order:

IllustrationBrief description of the operations performed
The detected crack should be carefully expanded.
The tool for this process must be selected depending on the thickness of the bulk layer. Most often, the expansion is carried out with the help of a "grinder", installing a disk for working with stone on it. Another tool suitable for expanding cracks (with a large layer thickness) can be a perforator with a special chisel attachment.
The crack must be expanded to 8÷10 mm, to the depth of the layer.
If necessary, the crack is limited by making transverse cuts along its edges - this will prevent it from growing in length.
Further, cut or removed areas must be well cleaned.
It is better to do this with a construction vacuum cleaner, since there should not be any remains of chipped mortar, small debris and dust inside.
The next step is a thorough priming of all surfaces of the crack to its full depth. It is even desirable to carry out this process two or three times, waiting for the previous layer to dry.
The primer will bind the material and create good adhesion for the repair mortar.
It is better to use a primer and a bulk mixture from the same manufacturer.
Further, it is necessary to dilute the required amount of the dry mixture of the self-leveling floor and pour the resulting solution into the prepared crack. The poured mortar must be leveled flush with the main surface.
If, after drying, the solution in the repair “patch” settles, you will have to walk along the crack with a primer, and then re-fill the roughness to the top with the solution.
After the solution has dried, the crack and its surrounding surface should be sanded.
To do this, you can use a “grinder” with an abrasive nozzle (“cup”) or a construction manual grater with an abrasive mesh or sandpaper stretched over it.

Screed floor repair

Defects such as local delamination and layer swelling require more extensive work, but can also be repaired without removing the entire bulk coating.

The sequence of work is not much different from the repair of cracks

The process is carried out according to the same principle as the repair of cracks, but has some nuances. Therefore, it is also worth considering step by step:

  • After the revision and detection of swollen and locally cracked areas of the self-leveling coating, before dismantling the layer, the damaged area should be marked.
  • When marking out, the area for future dismantling should include the entire area of ​​swelling or cracking, plus at least 100 mm of unaffected area deformation on each side. This must be done because of the weakening of the adhesive properties of the leveling layer and the base. If this recommendation is neglected, then the swelling of the coating may continue near the newly repaired area.

The swollen or cracked area will have to be removed completely, with the capture along the edges of "healthy" areas - at least 100 mm
  • Removal of the damaged area is carried out with the help of a "grinder", which cuts along the marking lines. The cuts will limit the growth of the deformed area.
  • Further, the self-leveling floor is crushed inside the cut out zone. This process should be done using a puncher, or manually using a chisel and hammer. The work must be done very carefully so as not to touch the “healthy” areas of the coating, otherwise you will have to unwittingly expand the repair area. In addition, care must be taken not to touch or damage the leveling roughing screed located below.
  • Angle grinder prices

    angle grinder

  • The next step is to prepare the dismantled area for a new pour. First, pieces of broken mortar are removed from the repair area. Next, the vacated area must be thoroughly vacuumed.
  • The next step is a thorough priming of the cleaned area. Especially abundantly and accurately, without "gaps", it is necessary to apply the composition to the edges of the zone, that is, to the ends of an intact self-leveling floor throughout the entire thickness. It is better to apply a primer in two or three layers, which should be well absorbed and dry.
  • Next, a solution is prepared for pouring the repaired floor segment. It should be identical to the main layer both in composition and consistency.
  • The mortar must be poured, taking into account its future shrinkage during curing. The amount of shrinkage is usually indicated by the manufacturer on the packaging of the mixture. In the case of a small thickness of the fill layer, the recommendations can be neglected. But if the solution is poured to a thickness of 70 ÷ 80 mm, it is advisable to immediately accurately calculate the shrinkage, based on the instructions.
  • To fill a thick layer, taking into account future shrinkage along the perimeter of the area to be poured, it is necessary to equip a low formwork made of plywood or wooden slats.
  • Then the filling is done.
  • After the mortar hardens, the formwork is removed.
  • Some craftsmen install formwork inside the perimeter of the repaired segment, on a rough screed, from thin plywood 3 ÷ 4 mm. Thus, after the removal of the formwork elements, a small gap is formed between the main floor layer and the repair one. A twine is laid and deepened into the formed seams, after which they are poured with the same solution. In this case, the mortar in the gaps must be poured to a depth of at least 5 mm above the laid twine.
  • After the mortar has dried and hardened, the repaired area, as well as the floor surface around it, are sanded. At the same time, the floor area processed by grinding should be periodically checked using a building level for horizontalness.

Before laying on the decorative finishing material, the protruding excess of the damper tape installed along the perimeter of the floor is cut off. And then a primer is applied to the entire surface.

* * * * * * *

So, we found out that the reasons for the appearance of cracks and swellings are primarily violations of the rules established by the technology. Therefore, having decided to level the floor on your own, you must strictly follow the recommendations of the mixture manufacturer - from preparing the base and mixing the solution, ending with pouring and distributing it over the rough screed.

If professionals are invited to perform this work, then you should not choose a random team of builders. It is better to turn to trusted companies that have been doing similar work for a long time. In addition, qualified private builders-finishers provide their services, who can provide video and photo evidence of their skills. And then with a high degree of probability it will be possible to hope that repair work on the self-leveling floor will not be required at all.

The video below will supplement the informational content of the article:

Video: Floor repair techniques

OOO "PolyTek System" 636

BY TYPE

Bulk floor in the apartment

Among floor coverings, used in the apartment, self-leveling floors are popular today, overshadowing even the laminate and tiles that were previously in demand. In their favor are such facts as:

  • abrasive resistance;
  • a variety of design solutions for apartments;
  • long service life.
In apartments, three types of coating are most often applied:
  • epoxy flooring;
  • polyurethane flooring;
  • cement-acrylic;
  • methyl methacrylate.
Epoxy resins are highly decorative. Floors can be matte or glossy, three-dimensional or backlit. The coating is resistant to moisture and household chemicals. An attractive price combined with high wear resistance has made this type of self-leveling floor one of the most popular among customers. Polyurethane floors, as well as epoxy floors, are durable, not afraid of moisture and chemicals, and resistant to abrasion. Cement-acrylic self-leveling floors are durable, non-slip surface, resistant to moisture. Most often used in the bathroom, toilet or kitchen. Methyl methacrylate self-leveling floor has a short hardening period of the layer, ready for use in 2-3 hours.

Benefits of using a self-leveling floor in an apartment

As a floor covering apartments self-leveling floor is used not by chance. Among its main advantages, customers and specialists distinguish:

  • durability of the material (at least 15 years, with a thick layer - more than 30 years);
  • versatility (can be used as an independent coating (in combination with the "warm floor" system), as a base for a laminate or carpet);
  • tightness (moisture does not penetrate into its structure, bacteria dangerous to health do not start);
  • the presence of fungicidal additives;
  • strength (may be damaged by strong point mechanical impact);
  • a wide range of colors to enhance the design.

Disadvantages of bulk coating

With a large number of pluses, self-leveling floors at home are not without minuses:
  • long and laborious preparation of the base;
  • it is recommended to use with a water system "warm floor";
  • high cost (taking into account the materials used);
  • strict adherence to technology.

Filling the self-leveling floor in the apartment

The technology of filling the self-leveling floor in the house experts verified to the smallest detail. A slight deviation from the technology will lead to the rapid arrival of the coating in an emergency state. The result of violations is the repair of self-leveling floors, which is only slightly inferior in price to the original filling. The work should be carried out by professionals, but it is better for the owner of the dwelling to know their order in order to be able to control it.

Self-leveling floors are poured onto a cement or concrete screed. It is necessary to carry out the dismantling of old coatings, leveling and repairing the old screed. Next, the floor screed is preliminarily, qualitatively cleaned of all types of contaminants, primarily oil or paint stains. From this, the quality of styling depends quite strongly. To improve the adhesion of the polymer mixture to the screed, the latter is covered with a primer layer. Beacons are installed on the floor. Then the composition of the self-leveling floor is distributed from the far corner of the wall to the exit from the room, its amount is calculated in advance, even when preparations are underway.

It is important to use quality materials correctly, observe technology and time frames in work. To create a flat surface, so that it is free of defects, it is recommended to install beacons on the very surface of the floor and at the base of the walls. Masters should not allow the formation of air bubbles on the surface. After solidification, they lead to serious defects, not to mention the fact that the expensive composition will be damaged.

Repair of polymer self-leveling floors

Loss of bulk polymer coating its performance may occur as a result of long-term operation or due to a violation of the filling technology. In the first case, due to high strength and long service life, the surface simply loses its attractive appearance. To update it, you just need to sand the coating and apply a new thin polymer layer. This work is done quickly and is relatively inexpensive.

More difficult to work if the resulting defects are associated with a violation of the pouring technology. When performing repairs, the technology that is necessary when pouring the coating in a residential area is strictly observed. The materials that are used in this case must match those that were originally used to improve adhesion.

Where to begin

Repair of self-leveling polymer coatings in apartments should begin with a thorough check to find out:
  • how much floor area is damaged;
  • what caused the defect;
  • how many layers will need to be replaced during the repair.
If the damaged area is large, and the reason for them was the incorrect installation of the layers during pouring, it is more profitable to consider the option of dismantling the coating and pouring a new one in compliance with the technology and the choice of high-quality materials. If the defects are minor, and they can be simply leveled, then floor repair is the best choice. The main thing is to entrust it to qualified specialists. PoliTek System LLC performs repairs of polymer self-leveling floors in residential premises with a guarantee, which is especially important when choosing a contractor.

Types of defects

The most common damage to poured concrete and epoxy floors caused by improper pouring:
  • cracks;
  • swelling and tubercles;
  • color changes (whitening);
  • delamination.

Stages of self-leveling floors repair

Restoration of self-leveling flooring in residential premises is carried out by the specialists of Politek System LLC as follows:
  • Examine the floor in the room and identify defects.
  • In case of swelling, cracks, discoloration, the upper polymer layer is dismantled with a perforator (so that there are no delaminations), the surface is prepared, a primer is applied, and a new polymer layer is poured last.
  • If cracks are found, work is carried out in a similar manner. A feature of the restoration of the coating in case of cracks is the study of the depth of damage.
  • It is necessary to dismantle all layers. Laying a new coating on a dismantled site is carried out in compliance with the technology for each level.
  • Peeling is a defect that provides for the most difficult repair, since not only the polymer coating can be separated, but also all layers, including the screed, to the base.

Repair of self-leveling polymer floors in case of peeling

If this type of defect is detected, an investigation is carried out, allowing you to determine which layers need to be restored. At the same stage, the area of ​​damage is determined. Often it turns out that the areas located near the defect have the same problem. Soon they will need the same repairs. In this case, it is more expedient to remove the entire coating laid in violation of the technology, which led to the formation of problems.

Such repairs are not cheap pleasure, and for its implementation it is necessary to invite professionals with experience in pouring self-leveling floor coverings and carrying out repair work

Ordering repairs in the company "PolyTek System" LLC

Politek System LLC provides services devices of self-leveling polymer floors on a concrete screed in apartments and repairs this type of coating. The main reason for contacting us is that highly qualified specialists who own the latest technologies and use modern equipment work in the state. In addition to experience and equipment, the company pays great attention to the quality of the materials used. Given that a slight violation of standards leads to the rapid formation of defects, specialists do not save on this item of expenditure. The floors filled with them will last for a dozen years, which will fully justify the costs incurred.

There were problems with the self-leveling floor - the company "PolyTek System" is ready to correct the situation and guarantee a quality result.
We are ready to offer you device (installation) of self-leveling floor in any premises. Our polymer-based materials can be poured in any room, they contain additives that give them decorative (for example, colored - tinted according to the RAL color chart, transparent for a pattern, like linoleum, marble) properties and other components that give them resistance to wear - no repair is needed for a long time.
Ideal foundation in order to pour the coating is a material such as concrete (or should be such as a concrete floor or cement screed). The thickness of the bulk coating very much depends on the basis on which it will be poured. The calculation can be done by our employees, call us and we will tell you the price of materials and the cost of work for your area. All items are in stock and available for delivery.

Updating the gloss, eliminating scratches and restoring the appearance of the polymer floor to its original.

Polymer self-leveling floors - a type of modern finish coating, widely used in various fields. Due to their high aesthetics, they are used for decoration of public spaces: offices, trading floors, exhibition halls, lobbies, etc. Strength and durability make them an ideal solution for the industrial sector, however, it is necessary to consider the expediency of their use for finishing floors in warehouses and workshops, since they are quite expensive.

Name of works price of works price of materials
Contouring of defective areas (including gouging, clearing for laying the Mapei high flow repair compound and epoxy repair coating) sanding sq. m. 300.00
Preparing the concrete base for laying the Mapei High Flow repair kit. Roughness device with a puncher with 5 mm grooves. sq. m. 300.00
Laying of repair mix Mapey up to 20 mm thick. Wetting of concrete. sq. m. 800.00 1400
Laying of polymer concrete with a strip of thickness. 10mm along def. Seam m. 500.00 200
Repair of cracks in the floor slab with jointing, filling of cracks with filling with epoxy composition. 500.00 200
Application of epoxy repair coating, sanding sq. m. 2 500.00 1000
Repair of the expansion joint of the concrete floor with a polymeric repair compound with re-cutting of the expansion joint and filling it with polyurethane sealant m.p. 750.00 300
Repair of concrete floor cracks with a polymer repair compound 20-50 mm wide, m.p. 1,000.00 600
Repair of potholes and pits in concrete pcs. 400.00 200
Repair of small cracks in concrete and prevention of spalling. sq. m. 550.00 100
Repair of cavities and small holes in concrete. sq. m. 700.00 200
Repair of a polymeric floor - delaminations of sq. m. 1,500.00
Repair of worn out topping - wear of topping sq. m. 450.00 300
Renovation of the polymer floor - wear sq. m. 550.00 500
Repair of concrete floor delaminations with polymers of thickness. 5mm. sq. m. 1 500.00 2000

Coatings of this type are produced on the basis of polyurethane, epoxy or methyl methacrylate resins. Floors of all presented categories differ in excellent technical characteristics. However, even such coatings sometimes require repair of polymer self-leveling floors, which will be able to perform the specialists of the company "SOYUZ".

Restoration of polymer floors with varnishes and mastics

The most common problem in the operation of polymer floors is loss of gloss and deterioration of the appearance of the coating . To restore them, special varnishes and mastics are used, presented on the modern market with a fairly large assortment. Excellent results provide mastics "Selbstglanz". These products form a high-strength film on the surface, which protects the floor from damage, guarantees an anti-slip effect and greatly facilitates the maintenance of polymer coatings.

It can be done with matt mastic or high-gloss Selbstglanz mastic, which after application forms a film resistant to mechanical damage. You can restore the shine and aesthetics of the coatings with the help of CITRIC and Prosept Multipower Polish detergent concentrates. In addition to the design function, these tools also perform a practical task, restoring the protective layer of coatings and extending the service life of self-leveling floors.

Repair of polymer floors in almost all cases, it is produced using two-component protective varnishes. Specialists of SOYUZ use coating grades that are safe for health, the advantages of which include quick drying, absence of a strong odor, high wear resistance, resistance to moisture and mechanical damage, as well as excellent decorative properties. Complicated coating damage and causes of their appearance Despite the presence on the modern market of a huge number of various mixtures of the highest quality, the appearance of serious defects on the surface of finished coatings is a fairly common phenomenon. The reason for the damage in most cases is the low qualification level of the performers.

Self-leveling floor repair may be needed if the following defects are detected: delamination with the top layer of concrete screed. The occurrence of this defect is a characteristic phenomenon in violation of the rules for pouring a concrete screed. Under the influence of mechanical loads, a more durable top layer exfoliates from a weak base subject to movement; delamination from the ground layer.

Repair of a polymer self-leveling floor becomes inevitable in case of violation of the drying time of the primer layer, as well as application to a surface contaminated with dust or oil, or an excessively wet base; delamination of a polymer coating with a primer base. The cause of the defect is a gross violation of the mixture pouring technology. Delamination of this type most often occurs in poorly polished areas, as well as in cases where pouring was carried out on a contaminated or wet base.

Besides, repair of epoxy and polyurethane resin floors may be needed when cracks, chips and potholes form on the surface.

Was before renovation Okay store on Leninsky pr.101


Became after repair

industrial floor repair

repair of self-leveling floors, price

If serious damage is detected, which includes all types of peeling of the polymer layer, industrial floor repair requires the removal of the damaged coating, after which the base is cleaned and primed, as well as the site is filled with a repair mixture. In cases where the cause of damage is the low strength of the screed, the optimal solution is a complete reconstruction of the floor with the removal of the polymer layer and the concrete base. After that, our specialists will fill the screed and apply a polymer coating in full compliance with the technology.

The cost of repairing polymer floors in this case, it will include the cost of pouring a new coating, as well as dismantling the old one. In case of minor damage associated with the wear of the coating, it is possible to apply a new thin layer of the mixture. At the finishing stage, specialists apply varnish and mastics, which guarantee the protection of the coating from loss of gloss and aesthetics. The SOYUZ company guarantees the high quality of restoration work and the efficiency of their implementation. We cooperate with leading manufacturers of polymer floors, which means that we know absolutely everything about such coatings. Our specialists will repair of self-leveling floors, price which will pleasantly surprise you. Call us, we will return beauty and reliability to polymer floors!

At the beginning of the installation of polymer self-leveling floors, it is important to choose the right material and strictly follow the technology of laying polymer coatings.

A quality approach is the key to a long and trouble-free operation of the floor. If these requirements are not observed, premature wear and destruction of the base is possible. And special attention should be paid to the re-installation of self-leveling floors and the installation of polymer coatings.

Violation of the structure of self-leveling polymer floors for industrial, sports purposes.

1) Detachment of the topcoat from the base, “bunit” coating:

  • Base waterproofing not done, water intrusion
  • Low grade concrete of the underlying base
  • Installation of self-leveling floors on the base with humidity exceeding 4%
  • the presence of oil stains and other contaminants on the substrate surface

Eliminate the cause of the appearance of moisture and dismantle the problem area, strengthen the bases with materials impregnated for deep penetration, and repeat the pouring of a new self-leveling floor at the site of the defect.

2) Potholes and cracks on the base finish

  • The resulting cracks in the base are repeated on the finish coating

locally or completely

It is necessary to make a base crack jointing, then prime and fill with a polymer composition with the addition of quartz sand and a self-leveling floor.

3) Abrasion and premature wear

  • Incorrect choice of top coat in service load areas

Options for the elimination and repair of self-leveling floors:

Selection of a coating that meets the requirements for operational loads and refilling of the coating.

4) Formation of craters and small through holes

  • The installation of polymer floors was carried out without a primer or an insufficient amount of material was applied, which requires complete sealing the pores of the base (dry places remained).
  • Poor-quality rolling with a needle aeration roller.

Options for the elimination and repair of self-leveling floors:

5) The appearance of small bubbles

  • A large amount of air formed in the composition of the polymer coating
  • Poor-quality rolling with a needle aeration roller
  • Also porous concrete base, screeds.

Options for the elimination and repair of self-leveling floors: Locally or completely

Perform the sanding method in problem areas or on the entire surface of the coating, prime, putty and re-apply the polymer coating.

6) Non-uniform surface

  • Ingress of water or moisture during installation of the coating

Dismantle the problem area, dry and refill the coating.

7) Sticky base surface after complete polymerization.

  • Poorly or poorly mixed components.
  • The self-leveling floor was installed with violations when mixing components (A and B) in the proportions of resin and hardener.
  • Also, a wet base or water ingress leads to non-curing of the polymer coating.

Options for the elimination and repair of self-leveling floors: Locally or completely.

Dismantling problem areas and refilling the coating.

Price, terms, conditions, guarantee

Name of service Period of execution Price RUB/m2 Guarantee for the work performed

Repair of self-leveling polymer floors

from 1 day to 1 week (depending on area)

depends on coverage, request a quote via the form below * 2 year

* - there is a discount for an area over 100 m2, the final price is negotiated with the manager after you fill out the order form.

Operation during work: Not

For the entire period of work on the installation of polymer floors, there should not be unauthorized persons at the facility except for the company's specialists.

Environmental friendliness: Yes

All materials used are certified by Sanepidnadzor. In the state of complete curing, the materials do not pose any health hazard. But in the liquid state, the materials have chemically volatile substances and when working with materials, standard chemical protection means should be used.

Start of operation: after 15 hours

Access to the premises is allowed 15 hours after applying the last layer of polymer. But strictly after the company's specialists give their permission for this.

Efficiency of the beginning of works: Yes

The deadlines for the commencement of work after the signing of the contract and payment of the advance part will begin on the fifth day from the date of receipt of funds to the contractor's settlement account.

Order for installation work you can make it on the company's website or by contacting the contact number indicated on the website, as well as leave a request in this case, after reviewing your request, the company's managers will contact you